How to control the color difference of injection molding products?

- May 06, 2019-


How to control the color difference of injection molding products?


  Chromatic aberration is a common defect in injection molding. It is not uncommon for the injection molding machine to be scrapped in batches due to the difference in color of the matching parts. There are many factors affecting chromatic aberration, including raw material resin, color masterbatch (or toner), mixing of color masterbatch with raw materials, injection molding process, injection molding machine, mold, etc. Because of the wide range of exposure, color difference control technology is also recognized as difficult in injection molding. Master one of the techniques. Asia Billion mould and Plastic is based on our practical experience. We generally control the color difference from the following six aspects.

 

    1. Eliminate the influence of injection molding machine and mold factors

 

    To select an injection molding machine with the same capacity as the injection molding product, it is best to replace the equipment if there is a problem with the dead angle of the injection molding machine. For the mold casting system, the exhaust groove, etc., the color difference can be solved by the maintenance mold of the corresponding part of the mold. The injection molding machine and mold problems must be solved before the production can be organized to reduce the complexity of the problem.

 

    2. Eliminate the influence of raw resin and color masterbatch

 

    Controlling raw materials is the key to completely solving chromatic aberrations. Therefore, especially in the production of light-colored articles, the significant influence of the difference in thermal stability of the raw material resin on the color fluctuation of the product cannot be ignored.

 

    Since most injection molding manufacturers do not produce plastic masterbatch or color masterbatch themselves, the focus can be on production management and raw material inspection. That is to strengthen the inspection of raw materials into the warehouse; the same product in production should be produced by the same manufacturer, the same brand masterbatch and color masterbatch;

 

    For color masterbatch, we must carry out sampling test color before mass production, both the same as the last proofreading, but also in this comparison, if the color difference is not big, can be considered qualified, as the batch color master has a slight color difference, can be The color masterbatch is remixed and used again to reduce the chromatic aberration caused by the uneven mixing of the color masterbatch itself. At the same time, we also need to focus on the thermal stability of the raw material resin and color masterbatch. For the poor thermal stability, we recommend that the manufacturer exchange.

 

    3. Eliminate the influence of uneven mixing of masterbatch and masterbatch

 

    Poor mixing of the plastic masterbatch with the color masterbatch will also make the color of the product change. After the masterbatch and the color masterbatch are mechanically mixed, when the hopper is fed into the hopper through the lower suction, the color masterbatch is separated from the masterbatch due to the action of static electricity, and is easily adsorbed on the hopper wall, which is bound to cause a change in the amount of the masterbatch during the injection molding cycle, thereby generating Color difference.

 

    In this case, the raw material can be sucked into the hopper and then manually stirred. For the addition of toner to produce colored products, the most effective way is to not use the suction machine, but use a hot air dryer to manually prevent the color difference caused by the separation of the toner from the masterbatch.

 

    4. Reduce the influence of barrel temperature on chromatic aberration

 

    In production, it is often encountered that a certain heating coil is damaged or the heating control part is out of control and the burning temperature causes a drastic change in the temperature of the barrel to cause chromatic aberration. The color difference caused by this kind of reason is easy to judge. Generally, the heating ring damages the chromatic aberration and the plasticization unevenness is accompanied by the aging. The heating control part is out of control and the long burning is often accompanied by product spot, severe discoloration or even coking. Therefore, the heating part should be inspected frequently during production, and it is found that the heating part is damaged or out of control and replaced in time to reduce the occurrence of such chromatic aberration.

 

    5, reduce the impact of the injection molding process adjustment

 

    When the non-color difference reason needs to adjust the injection molding process parameters, the injection temperature, back pressure, injection cycle and color masterbatch addition amount should not be changed as much as possible. At the same time, it is necessary to observe the influence of the process parameter change on the color. If the color difference is found, it should be adjusted in time.

 

    Avoid using high injection speed, high back pressure and other injection molding processes that cause strong shearing to prevent chromatic aberration caused by local overheating or thermal decomposition. Strictly control the temperature of each heating section of the barrel, especially the nozzle and the heating part next to the nozzle.

 

    6. Grasp the influence of barrel temperature and color masterbatch on product color change

 

    It is also necessary to know the trend of the color of the product as a function of temperature and color masterbatch before performing the color difference adjustment. Different color masterbatch varies with the temperature or color masterbatch of the product, and the color change law of the product is different. The color change process can be used to determine the law of change.

 

    Asia Billion can help you achieve high precision, high appearance requirements of molds and injection molded products, if you have any questions, please do not hesitate to contact us directly at sales@ab-industry.com. website: www.ab-industry.com 



Previous:How to do the first level maintenance of plastic mold ? Next:The characteristics of liquid silicone rubber injection molding machine